Aluminum is difficult to polish, as it is soft and the melting temperature is low. Too high temperatures will change the lattice structure of the aluminum, which can have impacts on further processing of the aluminum. Therefore different strategies and aluminas have to be applied. Almatis offers varius grades to fullfil the customers needs.

Hard

PSG 125

Alumina with top cut of 125 μm for heavy cutting compound and better pre-finishing compared to PSG 100.

PSG 140

Alumina with top cut of 90 μm for heavy cutting compound for good preperation of surface for the finishing process.

PSG 150

Ground alumina with top cut of 125 μm for cutting compounds.

PSG 300

Ground alumina with top cut of 40 μm for cutting compounds.

Medium

A 2

Unground alumina with top cut of 150 μm for heavy cutting compounds.

A 2-325 CR

Ground Alumina with special controlled top cut at 45 μm / 325 mesh for cutting compounds.

Soft

RAPOL140

Alumina with SSA of 4m2/g and a top cut of 90μm for high cutting compounds for metal surfaces.?

RAPOL 100

Alumina with SSA of 3,5m2/g and a top cut of 200μm for high cutting compounds as well as aluminum surfaces.